斷裂伸長率 | 500% | 拉伸強度 | 29MPa | 密度 | 0.956g/cm3 |
熔體流動速率 | 0.044g/10min | 規格級別 | 薄膜級 | 缺口沖擊強度 | 30 |
|
產品簡述
斷裂伸長率 | 500% | 拉伸強度 | 29MPa | 密度 | 0.956g/cm3 |
熔體流動速率 | 0.044g/10min | 規格級別 | 薄膜級 | 缺口沖擊強度 | 30 |
詳細數據
訂購指南
性能項目 | 試驗條件[狀態] | 測試方法 | 測試數據 | 數據單位 |
密度 | ASTM D-1505 | 0.956 | g/cm3 | |
Dart Drop沖擊強度 | ASTM D-1709 | >200 | g | |
Lzod缺口沖擊強度 | ASTM D-256 | >30 | kg.cm/cm | |
撕裂強度(MD) | ASTM D-882 | 6 | kg/cm2 | |
撕裂強度(TD) | ASTM D-882 | 200 | kg/cm2 | |
斷裂拉伸強度 | ASTM D-638 | 300 | kg/cm2 | |
屈服拉伸強度 | ASTM D-638 | 230 | kg/cm2 | |
Dart Drop沖擊強度 | ASTM D-1709 | >200 | g | |
斷裂拉伸強度(MD) | ASTM D-882 | 550 | kg/cm2 | |
斷裂拉伸強度(TD) | ASTM D-882 | 500 | kg/cm2 | |
維卡軟化點 | ASTM D-1525 | 124 | ℃ | |
彎曲模量 | ASTM D-747 | 10000 | kg/cm2 | |
熔點 | ASTM SGC | 131 | ℃ | |
洛氏硬度 | ASTM D-785 | 55 | R scale | |
熔融指數 | 190℃,2.16kg | ASTM D-1238 | 0.044 | g/10min |
ESCR | ASTM D-1693 | >1000 | Hrs | |
斷裂伸長率 | ASTM D-638 | 500 | % | |
伸長率(MD) | ASTM D-882 | 380 | % | |
伸長率(TD) | ASTM D-882 | 450 | % | |
脆化溫度 | ASTM D-746 | ℃ |