斷裂伸長率 | 580% | 拉伸強度 | 18MPa | 密度 | 0.922g/cm3 |
熔體流動速率 | 0.27g/10min | 缺口沖擊強度 | 260 |
|
產品簡述
斷裂伸長率 | 580% | 拉伸強度 | 18MPa | 密度 | 0.922g/cm3 |
熔體流動速率 | 0.27g/10min | 缺口沖擊強度 | 260 |
詳細數據
訂購指南
性能項目 | 試驗條件[狀態] | 測試方法 | 測試數據 | 數據單位 | ||
基本性能 | 熔體流動速率 | MI2.16 | ASTM D-1238 | 0.27 | g/10min | |
密度 | ASTM D-1505 | 0.922 | g/cm3 | |||
機械性能 | 1%伸長彈性系數 | MD | ASTM D-882B | 1700 | kg/cm2 | |
TD | ASTM D-882B | 1900 | kg/cm2 | |||
拉力斷裂強度 | MD | ASTM D-882B | 250 | kg/cm2 | ||
TD | ASTM D-882B | 220 | kg/cm2 | |||
拉力降伏強度 | ASTM D-638 | 95 | kg/cm2 | |||
抗撕裂性 | MD | ASTM D-1922 | 40 | N/mm | ||
TD | ASTM D-1922 | 50 | N/mm | |||
拉力斷裂伸長率 | ASTM D-638 | 700 | % | |||
硬度 | ASTM D-2240 | 51 | Shore D | |||
拉力斷裂強度 | ASTM D-638 | 190 | kg/cm2 | |||
拉力降伏強度 | MD | ASTM D-882B | 100 | kg/cm2 | ||
TD | ASTM D-882B | 100 | kg/cm2 | |||
摩擦系數 | ASTM D-1894 | >0.5 | ||||
拉力斷裂伸長率 | MD | ASTM D-882B | 380 | % | ||
TD | ASTM D-882B | 580 | % | |||
彎曲模量 | ASTM D-790 | 1500 | kg/cm2 | |||
落球行動強度 | ASTM D-1709 | 260 | g | |||
熱性能 | 維卡軟化點 | ASTM D-1525 | 96 | ℃ | ||
熔點 | DSC | 113 | ℃ | |||
脆化溫度 | ASTM D-746 | <-70 | ℃ | |||
其它性能 | 建設薄膜厚度 | 50~250 | µ | |||
濁度 | ASTM D-1003 | 15 | % | |||
光澤度 | ASTM D-2457 | 50 | % |