斷裂伸長率 | 580% | 拉伸強度 | 18MPa | 密度 | 0.921g/cm3 |
熔體流動速率 | 0.8g/10min | 用途級別 | 薄膜級,纖維 | 規(guī)格級別 | 薄膜 |
缺口沖擊強度 | 210 | 加工級別 | 注塑級 | 特性級別 | 增強級 |
|
產(chǎn)品簡述
斷裂伸長率 | 580% | 拉伸強度 | 18MPa | 密度 | 0.921g/cm3 |
熔體流動速率 | 0.8g/10min | 用途級別 | 薄膜級,纖維 | 規(guī)格級別 | 薄膜 |
缺口沖擊強度 | 210 | 加工級別 | 注塑級 | 特性級別 | 增強級 |
詳細(xì)數(shù)據(jù)
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | ASTM D-1505 | 0.921 | g/cm3 | ||
熔體流動速率 | ASTM D-1238 | 0.8 | g/10min | |||
機械性能 | 斷裂點伸長率 | MD | ASTM D-882B | 350 | % | |
TD | ASTM D-882B | 580 | % | |||
落球沖擊強度 | ASTM D-1709 | 210 | g | |||
降伏點強度 | MD | ASTM D-882B | 100 | kg/cm2 | ||
TD | ASTM D-882B | 110 | kg/cm2 | |||
1%伸長彈性系數(shù) | MD | ASTM D-882B | 1650 | kg/cm2 | ||
TD | ASTM D-882B | 1850 | kg/cm2 | |||
斷裂點強度 | MD | ASTM D-882B | 230 | kg/cm2 | ||
TD | ASTM D-882B | 190 | kg/cm2 | |||
熱性能 | 熔點 | DSC | 112 | ℃ | ||
軟化點 | ASTM D-1525 | 95 | ℃ | |||
脆化溫度 | ASTM D-746 | <-75 | ℃ | |||
其它性能 | 光澤度 | 45℃ | ASTM D-2457 | 60 | % | |
摩擦系數(shù) | ASTM D-1894 | >0.5 | ||||
濁度 | ASTM D-1003 | 8 | % | |||
抗撕裂性 | MD | ASTM D-1922 | 40 | N/mm | ||
TD | ASTM D-1922 | 50 | N/mm | |||
薄膜厚度 | 35-150 | ц |