斷裂伸長率 | 620% | 拉伸強度 | 19.6MPa | 密度 | 0.918g/cm3 |
熔體流動速率 | 2.3g/10min | 用途級別 | 薄膜級 | 規格級別 | 薄膜 |
缺口沖擊強度 | 96 | 加工級別 | 注塑級 | 特性級別 | 增強級 |
|
產品簡述
斷裂伸長率 | 620% | 拉伸強度 | 19.6MPa | 密度 | 0.918g/cm3 |
熔體流動速率 | 2.3g/10min | 用途級別 | 薄膜級 | 規格級別 | 薄膜 |
缺口沖擊強度 | 96 | 加工級別 | 注塑級 | 特性級別 | 增強級 |
詳細數據
訂購指南
性能項目 | 試驗條件[狀態] | 測試方法 | 測試數據 | 數據單位 | ||
基本性能 | 密度 | ASTM D-792 | 0.918 | g/cm3 | ||
熔體流動速率 | 190℃/2.16kg | ASTM D-1238 | 2.3 | g/10min | ||
薄膜厚度 | 50.8 | μ | ||||
機械性能 | 薄膜強度 | MD | ASTM D-882 | 140 | J/cm3 | |
TD | ASTM D-882 | 148 | J/cm3 | |||
切割模量 | MD | 2%正割 | ASTM D-882 | 166 | MPa | |
TD | 2%正割 | ASTM D-882 | 208 | MPa | ||
屈服拉伸強度 | MD | ASTM D-882 | 11.6 | MPa | ||
TD | ASTM D-882 | 11.0 | MPa | |||
斷裂拉伸強度 | MD | ASTM D-882 | 21.8 | MPa | ||
TD | ASTM D-882 | 19.6 | MPa | |||
斷裂伸長率 | MD | ASTM D-882 | 450 | % | ||
TD | ASTM D-882 | 620 | % | |||
落鏢沖擊強度 | ASTM D-1709 | 96 | g | |||
埃爾曼多夫撕裂強度 | MD | ASTM D-1922 | 320 | g | ||
TD | ASTM D-1922 | 190 | g | |||
熱性能 | 維卡軟化點 | ASTM D-1525 | 92.2 | ℃ | ||
熔點 | DSC | 108 | ℃ | |||
光學性能 | 光澤度 | 45° | ASTM D-2457 | 40 | ||
霧度 | ASTM D-1003 | 16 | % |